jbtsax
R.I.P. in memoriam 1947 - 2023
- Messages
- 8,985
- Location
- Beautiful Springville, Utah USA
I typically use contact cement and scratch/score the underside of the teflon sheet. It seems to do ok, but I am going to check out your method. I used to use thin tech cork for "regulation bars" as you call them, but I found it to be a bit noisy which is why I switched to .5 mm synthetic felt from JL Smith. I have been hammering it on a steel block to make it less compressible, but have found squeezing it with Knipex pliers does a cleaner job. I check how compressible a material is by closing my calipers as hard as I can and seeing how much the thickness changes.I like to use the thin synthetic felt for regulation bars, though I have some doubts about its long-term quietness. I've noticed that it seems to harden up over time (though most buffering materials do to some degree...or at least form a 'glaze'). Still something I'm looking at.
What d'you use to glue Teflon sheet on? I often find it comes off over time, no matter what process I use (roughing the surfaces, various glues etc.). The most longevity I've had out of it is by gluing a sheets of it to some very thin natural cork with an epoxy resin - and then glueing that to the key with the standard adhesives.