Thanks for the computer tip Mike.
Thanks for the computer tip Mike.
Just to be completely nerdy about it I've looked up the melting point of brass.
900 to 940 °C, 1652 to 1724 °F,
Using a hard solder runs the risk of over heating and your instrument becoming a puddle on the workbench.
Yes, I've done it. Brass goes read as you do it. Trick is to stop or severely reduce the heat as soon as the solder melts. Unlike soft solder where you're supposed to apply solder to a hot joint, here you should heat the solder as well.
Exactly. controlling that flame is the key. I've done thousands of repairs on horns using silver solder, and no melted or burned up brass yet. Now I'm not a professional tech making a living at this like the content experts here, but I've had personal success on horns in my own collection.
How about the surrounding lacquer and the adjoining guard feet, ribs, posts (on the body), etc. that ARE soft soldered? I can see using silver solder to repair a key off the saxophone where that degree of strength is required, but not on the body itself.
Griff and I have recommended the procedure used by professional repair techs everywhere and in the factories themselves when the instruments are manufactured. Beyond that, folks are free to use any method they choose.
If you are doing this for the first time, best to follow John, Griff and Colin's advice and use the low melt partial silver solder.
Is this JB weld somebody selling Araldite under a different name?........John
Is this JB weld somebody selling Araldite under a different name?........John
That is an excellent article with lots of detailed information. At Curt's suggestion I tried the "Tix" liquid flux for soft soldering and now I won't use anything else. It works great.Musicmedic.com (Bench Notes) has an article on all forms of Soldering, and also sells the stuff required.
The longevity of an epoxy repair is suspect. I'm not sure how it would cope with the stresses a saxophone goes through during temperature change, moisture and the vibrations during playing. Repairs have such a small surface area. It never seems to do what it says on the tin. A failure is bound to come at an inconvenient moment.
That is an excellent article with lots of detailed information. At Curt's suggestion I tried the "Tix" liquid flux for soft soldering and now I won't use anything else. It works great.
At the risk of raining on someone's parade, it should be said that using JB Weld, super glue, epoxy, etc. makes the correct repair (ie. soldering) at a repair shop more time consuming and expensive because the parts have to be separated and completely cleaned before any work takes place. Que sera, sera. . . .

J&B is indeed American. Araldite is of course the UK "equivalent" product by another manufacturer.

The longevity of an epoxy repair is suspect. I'm not sure how it would cope with the stresses a saxophone goes through during temperature change, moisture and the vibrations during playing. Repairs have such a small surface area. It never seems to do what it says on the tin. A failure is bound to come at an inconvenient moment.