I recently watched an episode of wheeler dealers where an old broken plastic bumper was welded. They seemed to think plastic welding was a new thing. I've fixed stuff in the past with a soldering iron.
Your points are well taken. I don't know the difference in hardness between sheet brass and sheet nickel silver, but I do have some experience with the strength of nickel silver keys on clarinets and the bodies of metal clarinets. Perhaps @Dr G can share his expertise on the subject. It appears that the Wilmington alto is being marketed as a "student saxophone" because of its price point and it's "looks". The real test of the resistance of the body of the instrument to dents and bending will be how it holds up in Junior High Band class for the first 2 or 3 years of use.I think the phrase "much more rigid" is doing a lot of work there.
It's also laughable insomuch as there are far better ways to increase rigidity than mucking about with a limited range of materials.
For example - it looks like the sax has a bog-standard triple-point bell brace. You could make the bell and bottom bow out of nickel silver as thick as you like within reason - but it would still never be as rigid as if the bell brace was a four-pointer (with an additional arm across the body).
If you really wanted to go the whole hog you could put a smaller brace further down the bell. Then it'd be really rigid.
At the sort of thickness of metal found on sax bodies, claims of material rigidity are just so much marketing w**k.
Your points are well taken. I don't know the difference in hardness between sheet brass and sheet nickel silver, but I do have some experience with the strength of nickel silver keys on clarinets and the bodies of metal clarinets. Perhaps @Dr G can share his expertise on the subject. It appears that the Wilmington alto is being marketed as a "student saxophone" because of its price point and it's "looks". The real test of the resistance of the body of the instrument to dents and bending will be how it holds up in Junior High Band class for the first 2 or 3 years of use.
Drop a horn of plastic, and make sure to pick up all the pieces for your repairman to glue together.It's a bit complicated. Hardness isn't the same as strength, which isn't the same as toughness.
And then you have to factor in the type of alloy. Some brasses are soft, some are hard - likewise nickel silver alloys. And then there's annealing to be factored in.
But in general terms nickel keys are more resistant to bending - but they're more likely to snap.
Out in the real world none of this makes that much difference for our purposes. If you drop a brass horn from three feet up, it's going to suffer as much as if it were made from nickel silver. The bottom bow will dent, the bell will twist and the body will bend from the bell brace upwards.
It's only when you start to introduce mechanical stiffness that you'll see meaningful results (such as the four-point bell brace or ribbed construction).
I'm surprised Yamaha haven't gone there.Drop a horn of plastic, and make sure to pick up all the pieces for your repairman to glue together.